| Chemical base | 1-component, moisture cure, thixotropic |
|---|---|
| Colour | Yellow |
| Cure | Tack-free 60–120 min; 24–48 h at room temperature, heat optional |
| Hardness | 67 Shore A |
| Operating temperature | -40 to +120 °C |
| Elongation at break | 300 % |