Thermal management: Bectron® materials that conduct heat

When a component has to give off heat through the material around it, thermal conductivity becomes the first column to read. The table lists every Bectron® product whose TDS gives 0.5 W/m·K or more, across potting compounds and adhesives, sorted by that value.

Nozzle laying a thermal gap-filler bead on a plate
Nozzle laying a thermal gap-filler bead on a plate. Image: ELANTAS Europe

Thermal conductivity (W/m·K): how to read the table

Sort by the W/m·K column first, then read cure and hardness for the products that reach your figure. A potting compound or an adhesive in the table also encapsulates or bonds.

Thermal conductivity
0.96 W/m·K
Chemical base
Epoxy resin
Hardness
Shore D 82

Schematic: through the same layer, heat flow scales with k.

Thermal conductivity from the TDS

Tab. 1≥ 0.5 W/m·K, highest first · 7
CodeChemical baseThermal conductivityHardnessOperating temperature
EP 5504 Epoxy resin0.96 W/m·KShore D 82Max. temperature 155 °C / 20,000 h
SG 75L2-30 Silicone (2-component, addition cure)0.90 W/mK–-50 °C to +180 °C
PU 4539 Polyurethane (2-component, filled)0.7 W/mK56 Shore A–
PU 4527 Polyurethane (2-component)0.56 W/mK40 ± 5 Shore D (ISO 868)–
PU 4526 Two-component polyurethane, with Hardener Bectron PH 49120.55–0.70 W/m·K (25 °C, ASTM C 518)35–45 Shore D/15 (25 °C, ASTM D 2240)-30 to +130 °C
SK 75V2-45 Two-component addition cure silicone, with crosslinker Bectron SH 79V2-45, Pt catalyst0.54 W/m·K45 Shore A-55 to +200 °C
PB 4540 Polybutadiene0.50 W/m·K43 A–

Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).

Related

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice

Contact directly

Alexandru Nichifor
Sales & technical support

+40 771 709 622

nichiforlx@nalteksolutions.com

Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298