Melting resins (hot melt): 10 ELANTAS Bectron® materials

10 Bectron® melting resins (hot melt) from ELANTAS Europe: one-part resins that set on cooling. The table gives base, viscosity, cure, operating temperature and UL 94 where the ELANTAS datasheet states them. Where a cell shows a dash, ask us for the TDS. For the application temperature, see Melting resins (hot melt).

Two test boards thick-film coated with Bectron® melting resin, translucent yellow-green and black
Image: ELANTAS Europe
Tab. 1Melting resins (hot melt) · 10
CodeBaseViscosityOperating temperatureUL 94
MR 3402 Polyolefin resin (1-component hot melt)8,500 ± 1,000 mPa·s (DIN 53018, 190 °C)-40 to +125 °C–
MR 3404 Polyolefin resin-based thermoplastic700–1,500 mPa·s (180 °C, PP25, DIN 53019)-40 °C to +105 °C–
MR 3404 H Polyolefin2,000 mPa·s @170 °CMax. operation temperature 100 °C–
MR 3405 Polyolefin (MR 34 series)2,100 mPa·s @190 °CMax. operation temperature 145 °C–
MR 3405 FR Polyolefin2,000 mPa·s @200 °C–V-0 (ELANTAS brochure)
MR 3405 H Polyolefin2,000 mPa·s @190 °C––
MR 3406 Polyolefin (1-component hot melt resin)520 ± 200 mPa·s (DIN 53018, 180 °C)-40 °C to +120 °C–
MR 3406 FR Hydrocarbon melting resin, polyolefin-based (1-component)800–1,250 mPa·s (180 °C, PP 25, DIN 53019)-40 to +125 °C (max. operation temperature 125 °C, 168 h)V-0
MR 3406 FR H Polyolefin2,500 mPa·s @190 °C–V-0 (ELANTAS brochure)
MR 3406 H Polyolefin2,000 mPa·s @180 °C-40/+125–

Also in this family, datasheet on request: MR 3402 H.

Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024). Datasheet PDFs.

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice

Contact directly

Alexandru Nichifor
Sales & technical support

+40 771 709 622

nichiforlx@nalteksolutions.com

Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298