VFP inks that print circuits

VFP Ink Technologies, a French ink maker, makes 13 inks for printed electronics: seven silver, two carbon, two UV-curing dielectric and two piezoelectric. They are printed on film, paper or glass to make membrane switches, printed heaters, touch panels, RFID and NFC antennas, in-mould parts and piezo sensors. We offer VFP Ink Technologies inks in Eastern Europe.

Used Bectron® printed-electronics inks? ELANTAS discontinued them in September 2026; the guide to replacing them names the VFP grade to trial for each Bectron® code.

VFP Ink Technologies image

Flexible film with a printed silver circuit

Image: VFP Ink Technologies

Ink ranges and process data

Tab. 1Ink ranges and process data
CodeInkPrintingCureResistivity / insulationSubstrates
SE Silver Electron Screen, 79–120 threads/cm 150 °C / 10 min; 130 °C / 30 min ≤ 15 mΩ/sq/mil Paper, PVC, PET, PC, treated polyester, glass, polyimide
SETF Silver Electron Thin Film Screen, 79–120 threads/cm 150 °C / 10 min; 130 °C / 30 min; NIR 4 s ≤ 150 mΩ/sq/mil Paper, PVC, PET, PC, treated polyester, glass, polyimide
SELEC Silver Electron Low Energy Curing Screen, 79–120 threads/cm 150 °C / 3 min; 120 °C / 5 min; NIR 2 s ≤ 15 mΩ/sq/mil Paper, cardboard, PET, treated polyester
LV-SELEC Low Viscosity Silver Electron Low Energy Curing Screen, 79–120 threads/cm 150 °C / 3 min; 120 °C / 5 min; NIR 2 s ≤ 12 mΩ/sq/mil Paper, cardboard, PET, treated polyester
SES Silver Electron Stretchable Screen, 77–90 threads/cm 150 °C / 10 min; 130 °C / 30 min; NIR 2 s < 10 mΩ/sq/mil on PET; < 50 after 20 % elongation on TPU; < 300 after thermoforming on PC PET, PC, polyurethane; thermoformable
FSE Flexography Silver Electron Flexo, anilox 12–16 BCM; or screen 150 °C / 10 min; 120 °C / 30 min; NIR 2 s ≤ 10 mΩ/sq/mil Paper, PVC, PET, PC, treated polyester, glass, polyimide
SECTR-I01 Silver Electron Chemically and Thermally Resistant, 2-component Screen, 79–120 threads/cm; 5–8 µm at 90 threads/cm 120 °C / 5 min (≤ 10 mΩ/sq/mil); 50 °C / 30 min gives ≤ 25 mΩ/sq/mil ≤ 10 mΩ/sq/mil Untreated and TCA-treated PET, paper; PC, polyimide or PVC depending on the TDS revision: confirm with VFP
CEL001 Carbon Electron 001 Screen, 79–120 threads/cm; prints over SE, SETF, FSE 120–150 °C / 3–5 min ≤ 120 Ω/sq/mil at 120 °C / 5 min Paper, cardboard, PET, treated polyester
CEL003 Carbon Electron 003 Screen, 79–120 threads/cm; prints over SELEC, LV-SELEC 120–150 °C / 3–5 min; NIR 2 s 120 Ω/sq/mil at 120 °C / 5 min Paper, cardboard, PET, treated polyester
ECV003 Dielectric Varnish-003 Screen, 79 or 90 threads/cm Broad-spectrum UV (mercury/xenon), > 300 mJ/cm²; peaks 359/365/380/383 nm Insulation > 2 TΩ; breakdown 4,000 V for 2 layers Paper, PET, PC, treated polyester
ECV004 Dielectric Varnish-004 Screen, 79 or 90 threads/cm Broad-spectrum UV (mercury/xenon), > 300 mJ/cm²; peaks 359/365/380/383 nm Insulation > 2 TΩ; breakdown 4,000 V for 2 layers Paper, PET, PC, treated polyester
PEUV Piezo Electron UV Screen, 79–90 threads/cm; 30 µm in 2 layers UV, mercury lamp, 300 mJ/cm² Piezoelectric d33 = 2 pC/N; poling 20 V/µm; Curie 130 °C Untreated and TCA-treated PET; prints over VFP silver; PFAS-free
PESOL Piezo Electron Solvent Screen, from 43 threads/cm; 30 µm in 2 layers 120 °C / 5 min Piezoelectric d33 = 8 pC/N; poling 20 V/µm; Curie 130 °C Untreated and TCA-treated PET; prints over VFP silver; PFAS-free

Source: the VFP Ink Technologies datasheet (TDS) of each grade; NIR drying and anilox values from VFP’s presentation of April 2026. Values are VFP’s; VFP advises a preliminary test on your substrate.

VFP SECTR-I01 two-component silver ink
VFP SECTR-I01 two-component silver ink
VFP Piezo Electron ink
VFP Piezo Electron ink

Which VFP inks for which device

Pick a device and read the stack from the film upward: each layer names the VFP ink that prints it. VFP names each of these applications; the ink for each layer is our reading of VFP’s datasheets. Every stack needs a print trial on your substrate, as VFP advises.

Pick the device
A key press closes the contact and the signal leaves on the silver track.
  1. 1SubstratePET
  2. 2SilverSELEC or LV-SELEC tracks
  3. 3CarbonCEL003 on the contacts
  4. 4ECV003 or ECV004 dielectric

With SE tracks, use CEL001.

Check your lamp before you add the dielectric. Which UV dryer, and how to check the dose · Hoenle UV Meter

Buying VFP inks through Naltek

Samples
100–500 g
Minimum order
1 kg per silver ink; 500 g per dielectric; other grades on request
Lead time
5–15 business days from order
Documents
TDS before you order; REACH declaration of conformity and SDS with each order
Prices
Quoted per inquiry
Support
Naltek is your first contact; VFP offers on-site technical support and training, at its site or yours
Compliance
REACH; RoHS 3 for the silver and carbon inks; all 13 printed-electronics grades are in VFP’s non-CMR category

VFP terms of sale, Article 3: delivery lead times are given for information only and without guarantee.

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice

Contact directly

Alexandru Nichifor
Sales & technical support

+40 771 709 622

nichiforlx@nalteksolutions.com

Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298