Melting resins (hot melt) for encapsulating electronics
The 10 Bectron® melting resins are applied molten and set as they cool, with no mixing and no cure schedule. The application temperature is the one the TDS gives for each product.
Melting resins (hot melt) for encapsulating electronics
Application temperature of a melting resin, and repair
Set the nozzle to the application temperature in the TDS. For MR 3406 that is 190–200 °C, with the reservoir at 170 °C for one day at most; 180 °C is only its viscosity reference. The resin can be melted off for repair. The hot-melt guide has the figures for MR 3406, MR 3406 FR and MR 3404.
- Nozzle
- 190–200 °C for MR 3406 (MR 3406 TDS)
- Reservoir
- 170 °C, one day at most
- Sets
- as it cools: no mixing, no cure schedule
- Repair
- the resin can be melted off
- Figures
- MR 3406, MR 3406 FR and MR 3404 in the hot-melt guide
Colours are schematic.
Pictures
Bectron® products and TDS values
| Code | Chemical base | Viscosity | Operating temperature |
|---|---|---|---|
| MR 3402 | Polyolefin resin (1-component hot melt) | 8,500 ± 1,000 mPa·s (DIN 53018, 190 °C) | -40 to +125 °C |
| MR 3404 | Polyolefin resin-based thermoplastic | 700–1,500 mPa·s (180 °C, PP25, DIN 53019) | -40 °C to +105 °C |
| MR 3404 H | Polyolefin | 2,000 mPa·s @170 °C | Max. operation temperature 100 °C |
| MR 3405 | Polyolefin (MR 34 series) | 2,100 mPa·s @190 °C | Max. operation temperature 145 °C |
| MR 3405 FR | Polyolefin | 2,000 mPa·s @200 °C | – |
| MR 3405 H | Polyolefin | 2,000 mPa·s @190 °C | – |
| MR 3406 | Polyolefin (1-component hot melt resin) | 520 ± 200 mPa·s (DIN 53018, 180 °C) | -40 °C to +120 °C |
| MR 3406 FR | Hydrocarbon melting resin, polyolefin-based (1-component) | 800–1,250 mPa·s (180 °C, PP 25, DIN 53019) | -40 to +125 °C (max. operation temperature 125 °C, 168 h) |
| MR 3406 FR H | Polyolefin | 2,500 mPa·s @190 °C | – |
| MR 3406 H | Polyolefin | 2,000 mPa·s @180 °C | -40/+125 |
Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).
How it is applied
| Thin film, selective | PL 4122-40, PL 1102, PT 4700 N | Selective spray or film-coating valve on a coating robot |
|---|---|---|
| Thick film, selective | PT 4600, PT 4601, PK 4340 | Bead or film dispensing; PT 4600 cures under UV, shadow areas by moisture |
| Melting resins | MR 3402, MR 3405, MR 3406 | Heated hot-melt application at the temperature the TDS gives |
Related
- Conformal coating vs potting for power electronics: what the datasheets show
- Hot-melt (melting resin) PCB coating: what application temperature?
- How to protect a PCB from condensation: coating options with datasheet values
- Thin-film vs thick-film conformal coating: solvent, cure and film build compared
- Potting and encapsulation
Ask for a sample, a TDS, a quote or a dose calculation
Tell us what you need. We reply within 24 hours, in Romanian or English.
Contact directly
Alexandru Nichifor
Sales & technical support
nichiforlx@
Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298