Hardeners, thinners and cleaners: 10 ELANTAS Bectron® materials

10 Bectron® auxiliaries from ELANTAS Europe: 4 hardeners and 5 thinners and cleaners. They belong to the potting compounds and coatings; the product pages name the pairing where the TDS gives it. Where a cell shows a dash, ask us for the TDS.

Tab. 1Hardeners · 4
CodeBaseViscosity
PH 4901 Polyurethane hardener (for transparent PU casting resins)250 ± 150 mPa·s (23 °C, DIN 53019)
PH 4912 Polyurethane hardener90–140 mPa·s (25 °C, ISO 3219)
PH 4913 Polyurethane hardener (filled PU casting compounds)27.5 ± 12.5 mPa·s (25 °C, DIN 53019)
PH 4918 Hardener for polybutadiene (PBD) potting resins1,200 ± 300 mPa·s (23 °C, DIN 53019)
Tab. 2Thinners and cleaners · 1
CodeBase
239 Organic solvent blend

More in this group (details on the product page): 217, 225, 300, AC 93.

Tab. 3Masking · 1
CodeBaseViscosityCure
AP 8100 1-component modified natural rubber based masking materialThixotropic (DIN 53018)about 1 h at room temperature (1 mm film); 6–10 h up to 3 mm

Also in this family, datasheet on request: PH 4916.

Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024). Datasheet PDFs.

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice

Contact directly

Alexandru Nichifor
Sales & technical support

+40 771 709 622

nichiforlx@nalteksolutions.com

Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298