Potting and encapsulation: 39 ELANTAS Bectron® materials

39 Bectron® potting compounds from ELANTAS Europe: 19 polyurethane, 7 silicone elastomer, 5 silicone gel, 3 epoxy and 5 polybutadiene. The tables give base, viscosity, cure, operating temperature and UL 94 where the ELANTAS datasheet states them. Where a cell shows a dash, ask us for the TDS. For polyurethane against silicone, see Potting and encapsulation.

Automotive control unit in a plastic housing, its circuit board encapsulated under clear potting compound
Image: ELANTAS Europe
Tab. 1Polyurethane · 16
CodeBaseViscosityCureOperating temperatureUL 94
PU 4501 Polyurethane (2-part, polyetherpolyol resin + aliphatic isocyanate hardener)––Temperature cycling -40/+125 °C–
PU 4512 Polyurethane (2-component, filled)900 mPa·s–––
PU 4513 Polyurethane (2-component, solvent-free)750 ± 150 mPa·s (DIN 53019, 25 °C)24 h at room temperature or 1–1.5 h at 90 °CThermal class 115 °C (IEC 216); flexible down to -40 °C–
PU 4515 Two-component polyurethane modified with polybutadiene, with Hardener Bectron PH 4912––-60 to +150 °C–
PU 4516 Polyurethane (2-component)310 ± 90 mPa·s (DIN 53019, 25 °C)36h @RT, 1h @90 °C––
PU 4519 Polyurethane (2-component, solvent-free)2,500 ± 500 mPa·s (DIN 53019, 25 °C)–––
PU 4522 Polyurethane (2-component liquid)1,800 ± 300 mPa·s mixed, 25 °C (resin 3,500 ± 300)6–8 h at room temperature or 0.5 h at 90 °C-40 °C to +125 °CV-0
PU 4526 Two-component polyurethane, with Hardener Bectron PH 49123,000–4,000 mPa·s mixed, 25 °C (resin 10,000–18,000)–-30 to +130 °CV-0 (File E116643, 5.5 mm)
PU 4527 Polyurethane (2-component)11,000 ± 1,600 mPa·s (DIN 53019, 25 °C)–––
PU 4528 Polyurethane (PU)4,000 mPa·s–––
PU 4532 Polyurethane (PU)700 mPa·s–––
PU 4533 Polyurethane (2-component, solvent-free)––-40 °C to +120 °C–
PU 4534 Polyurethane5,000 ± 1,000 mPa·s (resin)–-40 °C to +130 °CV-0
PU 4535 Polyurethane (2-component)550 ± 90 mPa·s (DIN 53019, 23 °C)–-40 °C to +120 °C–
PU 4537 Polyurethane (2-component)–16-24h @RT, 3-4h @80 °C–V-0
PU 4539 Polyurethane (2-component, filled)4,000 mPa·s––V-0

More in this group (details on the product page): PU 4518, PU 4520, PU 4521.

Tab. 2Silicone elastomer · 7
CodeBaseViscosityCureOperating temperatureUL 94
SK 75V1-35 Silicone (2-component, addition cure)990 mPa·s at 25 °C30 min at 90 °C or 1 h at 120 °C-40 °C to +200 °CV-0 (ELANTAS internal test)
SK 75V2-35 Silicone (2-component, addition cure)1,050 mPa·s at 25 °C12 h-50 °C to +180 °CV-1
SK 75V2-45 Two-component addition cure silicone, with crosslinker Bectron SH 79V2-45, Pt catalyst–24 h-55 to +200 °CV-0
SK 75V2-65 Silicone (2-component, addition cure)3,500 mPa·s at 25 °C24 h-40 °C to +200 °CV-0 (ELANTAS internal test)
SK 76V2-50 Silicone (2-component)2,600 mPa·s24 h-40 to +180 °C–
SK 76V2-75 Silicone (2-component, condensation cure)7,500 mPa·s at 25 °C6 h-40 °C to +180 °CV-1
SK 7502 Silicone–––HB
Tab. 3Silicone gel · 5
CodeBaseViscosityCureOperating temperatureUL 94
SG 75L2-30 Silicone (2-component, addition cure)10,500 mPa·s (mixed)48 h at room temperature or 2 h at 80 °C-50 °C to +180 °CV-0 (File E140720)
SG 75V1-15 Silicone (2-component, addition cure)3000 mPa*s24 h at room temperature; 30 min at 100 °C; 10 min at 150 °C-45 °C to +200 °C–
SG 75V1-60 Silicone Gel (2-component)350 mPa·s24 h-45 to +200 °CV-1 (ELANTAS internal test)
SG 75V1-70 Silicone–24h @25 °C––
SG 75V1-75 Silicone (2-component, addition cure)750–1,250 mPa·s mixed (25 °C)1.5 h at room temperature; 15 min at 60 °C; 5.5 min at 120 °C-40 °C to +180 °CHB (File E140720, 3 mm)
Tab. 4Epoxy · 3
CodeBaseViscosityCureOperating temperatureUL 94
EP 5502 Epoxy––Max. operation temperature +120 °C (no lower limit printed)–
EP 5503 Epoxy resin6000 ± 1500 mPa*s18 h-40 °C to +150 °C–
EP 5504 Epoxy resin2,700 mPa·s–Max. temperature 155 °C / 20,000 hV-0
Tab. 5Polybutadiene · 5
CodeBaseViscosityCureOperating temperatureUL 94
PB 3200 Polybutadiene900 ± 150 mPa*s24 h––
PB 3201 Polybutadiene7,500 ± 2,000 mPa·s (DIN 53019, D=7 s-1, 23 °C)48 h-60 °C to +150 °C–
PB 3251 Polybutadiene15000 ± 3000 mPa*s48 h-60 to +150 °C–
PB 3252 Polybutadiene2000 ± 500 mPa*s48 h-55 to +120 °C–
PB 4540 Polybutadiene–24h @25 °C, 20min @90 °C–V-0

Also in this family, datasheet on request: PB 3231, SG 7510 VP, SG 7511 VP, SK 7568, SK 7569, SK 7571.

Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024). Datasheet PDFs.

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice

Contact directly

Alexandru Nichifor
Sales & technical support

+40 771 709 622

nichiforlx@nalteksolutions.com

Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298