Adhesives and sealants for electronics assembly

The 14 Bectron® adhesives and sealants fix components and seal housings and covers. ELANTAS describes the SA 70 silicone series as designed for corrosion-sensitive devices. The table shows the values from the ELANTAS datasheets we have on file; ask for the current TDS before you qualify a product.

Adhesives and sealants: 14 products

Adhesives and sealants for electronics assembly

Formed-in-place gasket beads dispensed on a housing lid
Image: Naltek archive

Silicone sealants with a neutral cure for corrosion-sensitive parts

The SA 70 series are one-part silicones with a neutral (alkoxy) cure. The SA 70L1-30 TDS calls the product non-corrosive in contact with sensitive electronic parts and gives −55 to +200 °C. A 3 mm section cures in under 24 h at 23 °C and 55 % relative humidity; full bond strength comes after 5 days.

SA 70L1-30
one-part silicone, neutral (alkoxy) cure
Cure
a 3 mm section in under 24 h at 23 °C and 55 % relative humidity
Full bond strength
after 5 days

Pictures

Circuit board with clear adhesive securing a chip package and a crystal oscillator against vibration
Circuit board with clear adhesive securing a chip package and a crystal oscillator against vibration. Image: ELANTAS Europe

Bectron® products and TDS values

Tab. 1
CodeChemical baseViscosityCureOperating temperature
AR 4800 N 1-component, moisture cure2,400 mPa·sTack-free 60–120 min; 24–48 h at room temperature, heat optional-40 to +120 °C
AR 4820 N One-component polyurethane, moisture cure––-45 to +120 °C
AR 4822 N 1-component polyurethane, moisture cure15,000 ± 4,000 mPa·s (23 °C, D = 3 s⁻¹, DIN 53019)24 h at room temperature (≥ 50 % RH, up to 0.5 mm); for best adhesion 24 h at RT, then 24 h at 90 °C-45 to +120 °C
AR 4826 N 1-component, moisture cure, thixotropic–Tack-free 60–120 min; 24–48 h at room temperature, heat optional-40 to +120 °C
EP 5611 One-component modified epoxy, UV + heat dual cure, filled, thixotropic25,000–40,000 mPa·s (25 °C, DIN 53019, D = 50 s⁻¹)UV 1–3 s at 50 mW/cm² UVA (+30 min at 150 °C); heat only 30 min at 150 °C-40 to +150 °C (Insert 8, 09/2022)
EP 5620 One-component modified epoxy, heat cure, solvent-free800 ± 300 mPa·s (23 °C, DIN 53019, D = 3 s⁻¹)––
SA 70L1-30 One-component condensation cure silicone (Alkoxy), neutral cure44,000 mPa·sTack-free 2–10 min (23 °C, 55 % RH); cured < 24 h (3 mm)Temperature resistance -55 to +200 °C
SA 70L1-36 Silicone (1-part)3,200 mPa·s–-40/+200 °C
SA 70P1-15 Silicone (1-part)Paste–-40 to +200 °C
SA 70P1-30 Silicone (1-part)Paste36 hours at 23 °C (3mm thickness)-55 °C to +200 °C
SA 70P1-34 Silicone (1-part)Paste–-40 to +200 °C
SA 70P9-50 SiliconePaste–-55 to +160 °C
SA 70P9-60 Silicone (1-part)Paste24 hours at 25 °C (3 mm thickness)-55 °C to +200 °C
SA 70V1-36 Silicone––-55 °C to +200 °C

Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).

Related

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice

Contact directly

Alexandru Nichifor
Sales & technical support

+40 771 709 622

nichiforlx@nalteksolutions.com

Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298