Coatings that protect circuit boards, UV lamps that cure coatings, inks that print circuits

Naltek Solutions is a technical reseller in Gurghiu, Mureș, supplying electronics plants in Romania since 2021. Products from ELANTAS Bectron®, Hoenle AG and VFP.

Naltek Solutions is a technical reseller for electronics plants, based in Gurghiu, Mureș county. We are a Distribution partner of ELANTAS for Bectron® coatings, potting and adhesives in Romania. We also offer Hoenle AG UV curing systems in Romania and VFP Ink Technologies inks in Eastern Europe.

We help you choose the material and the curing equipment that fit your product’s requirements and evaluate the whole process around them: cost, process time and line speed. We run trials on your line, help with troubleshooting, calculate the UV dose, and measure it on site on request.

Circuit boards protected with Bectron® materials
Image: ELANTAS Europe

Product lines: ELANTAS Bectron®, Hoenle AG, VFP Ink Technologies

Compact Hoenle LED heads irradiating a small optical part, under violet light

Hoenle AG LED UV curing

18 LED curing systems, from a hand pen to a conveyor line

Hoenle AG builds LED curing systems, UV at 365–405 nm, from a hand pen to a conveyor line. We work out which unit reaches the UV dose in your coating’s datasheet.

You can check a lamp yourself in the UV dose calculator.

Used for: UV curing, Printed electronics

Flexible printed circuit: silver tracks under a green dielectric layer

VFP printed-electronics inks

13 silver, carbon, UV dielectric and piezoelectric inks

13 grades of silver, carbon, UV dielectric and piezoelectric ink, for membrane switches, printed heaters, touch panels and antennas.

Used for: Printed electronics

Applications

Each application page lists the Bectron® materials, Hoenle AG units and VFP inks that fit the process.

All applications

Supplying production lines at Romanian electronics plants since 2021, and taking part in R&D projects

We have supplied or sampled 7 plants in Romania.

We work under NDAs with several of our customers, so plants are not named here. References are available when the customer agrees.

All plant references About Naltek

Three plant references and our R&D work

We work under NDAs with several of our customers, so plants are not named here. References are available when the customer agrees.

  • R&D with automotive Tier-1 teams

    We take an active part in development projects of automotive Tier-1 teams: material trials and process tests, run together with our suppliers.

  • EMS plant in Romania

    Registered supplier since 2022, with repeat orders every year.

  • Electronics plant in Romania

    Conformal coating reordered every year since 2023.

  • Production-equipment supplier to electronics plants

    From sample to supply for a coating project. An urgent order in February 2025 was dispatched nine days after the purchase order.

Which Bectron® material for which job

When to use each family.

Seven Bectron® material types and the job each one fits.

  • Thin-film coating

    PL 4122, PL 1102, PL 1104

    The whole board, or large areas, needs a film applied by dip or spray, cured at room temperature or in an oven.

  • Thick-film coating, heat cure

    PK 4340

    You need 100 % solids and no VOC, more build on edges and components, support for components or a dam. An oven or IR cures it, with no lamp and no shadow problem.

  • Thick-film coating, UV cure

    PT 4600, PT 4700 N

    The line needs a cure in seconds. The lamp must reach the dose in the datasheet; in shadow areas moisture finishes the cure over the following days.

  • Polyurethane potting

    PU 4522, PU 4526

    A module in a housing needs full encapsulation with a harder two-component material. Polyurethane does not suit low-surface-energy plastics.

  • Silicone potting and gels

    SK, SG

    Power modules, thermal shock and the highest operating temperatures. Addition-cure grades can be inhibited.

  • Melting resin (hot melt)

    MR

    No mixing and no cure step: the resin sets on cooling, and you can melt it off for repair.

  • Silicone adhesive

    SA 70L1-30

    You seal or fix components on corrosion-sensitive assemblies without a primer.

Buying through Naltek

Support at your plant
UV dose measurement, process set-up and trials on your line are services we quote per inquiry.
Samples and small quantities
A factory pack can be a 30 kg pail when the trial needs 5 l. We help with samples and trial quantities. VFP samples are 100–500 g.
Payment
30 days; the first order is paid in advance.
Delivery from the manufacturer
Bectron®: 8 weeks from order; SA 70L1-30 in cartridges about 3 months.Hoenle AG standard units, accessories and spare parts: about 4–5 weeks from order. Custom systems: lead time per quote.VFP inks: 5–15 business days from order.We agree the delivery terms with you for each order.
Documents before you order
TDS and SDS before you order. Bectron® deliveries come with a certificate of analysis from ELANTAS.
Your NDA
We sign it before you share drawings or process data.
  • Support at your plant
    UV dose measurement, process set-up and trials on your line are services we quote per inquiry.
  • Samples and small quantities
    A factory pack can be a 30 kg pail when the trial needs 5 l. We help with samples and trial quantities. VFP samples are 100–500 g.
  • Payment
    30 days; the first order is paid in advance.
  • Delivery from the manufacturer
    Bectron®: 8 weeks from order; SA 70L1-30 in cartridges about 3 months.Hoenle AG standard units, accessories and spare parts: about 4–5 weeks from order. Custom systems: lead time per quote.VFP inks: 5–15 business days from order.We agree the delivery terms with you for each order.
  • Documents before you order
    TDS and SDS before you order. Bectron® deliveries come with a certificate of analysis from ELANTAS.
  • Your NDA
    We sign it before you share drawings or process data.

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice

Contact directly

Alexandru Nichifor
Sales & technical support

+40 771 709 622

nichiforlx@nalteksolutions.com

Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298