40 Bectron® conformal coatings from ELANTAS Europe: 15 thin-film and 25 thick-film grades. The tables give base, viscosity, cure, operating temperature and UL 94 where the ELANTAS datasheet states them. Where a cell shows a dash, ask us for the TDS. For thin film against thick film, see Conformal coating.
| Code | Base | Viscosity | Cure | Operating temperature | UL 94 |
|---|---|---|---|---|---|
| PL 1102 | Acrylic | 40 ± 15 s, 4 mm cup, 23 °C (≈ 50 mPa·s) | – | Temperature resistance 130 °C | V-0 (ELANTAS internal test) |
| PL 1104 | Acrylic | 40 ± 15 seconds flow time (DIN/EN/ISO 2431, 4mm cup, 23 °C) ≈ 50 mPa·s | – | -40 °C to +130 °C | – |
| PL 4122-37 | Polyurethane varnish | 40 ± 3 seconds (DIN/EN/ISO 2431, 4mm cup, 23 °C) ≈ 50 mPa·s | – | Temperature index 134 °C (IEC 60216) | V-0 (File E211569) |
| PL 4122-40 | Polyurethane varnish | 65 ± 5 seconds flow time (DIN/EN/ISO 2431, 4mm cup, 23 °C) ≈ 80 mPa·s | – | Temperature index 134 °C (IEC 60216) | V-0 (File E211569) |
| PL 4122-40P | Urethane/Alkyd | – | 16h @23 °C | – | V-0 |
| PL 4122-41 R | Urethane/Alkyd | 70 ± 20 mPa·s (DIN 53019, 23 °C, D=30 s-1) | – | – | V-0 (File E211569) |
| PL 4122-45 | Polyurethane varnish | 40 ± 3 s, 6 mm cup, 23 °C (≈ 240 mPa·s) | – | Temperature index 134 °C (IEC 60216) | V-0 (File E211569) |
| PL 4122-45T | PUR, stab. | – | 24h @25 °C, 30min @80 °C | – | V-0 |
| PL 4122-47 R | Urethane/Alkyd | 600 ± 150 mPa·s (DIN 53019, 23 °C, D=30 s-1) | 16h @23 °C | Temperature index 134 °C (IEC 60216) | V-0 (File E211569) |
| PL 5621D | Epoxy | 400 ± 250 mPa·s (DIN 53019) | – | -40 to +130 °C (short-term 160 °C) | V-0 (ELANTAS internal test) |
| PL 5622-250 | Epoxide | – | – | -40 °C to +150 °C | V-0 (TDS 2019, no file number) |
| SC 75V1-16 | Silicone | – | – | -40 °C to +200 °C | V-0 (ELANTAS internal test) |
| SC 76V1-20 | Silicone | – | 20 to 25 °C Room temperature; | -40 °C to +200 °C | V-0 (ELANTAS internal test) |
| SC 76V1-36 | Silicone (1-part, condensation cure, Alkoxy) | 3,100 mPa·s | 24 hours (3 mm thickness) | -55 °C to +200 °C | HB (ELANTAS internal test) |
| SDC 76V1-18 | Silicone | – | – | – | V-0 |
| Code | Base | Viscosity | Cure | Operating temperature | UL 94 |
|---|---|---|---|---|---|
| PK 4332 | Polyurethane (1-component) | 5,500 ± 1,000 mPa·s (DIN 53019, D=15 s-1, 23 °C) | 70-90 min | -60 °C to +125 °C | – |
| PK 4340 | One-component polyurethane duroplastic (encapsulated polyisocyanate), thixotropic | 8,000–11,000 mPa·s (23 °C, DIN 53019, D = 15 s⁻¹) | 90 °C: 30 min (TDS range 25–35 min), recommended by ELANTAS; 80 °C: 60 min (60–70) | -60 to +125 °C (temperature cycling) | – |
| PK 4342 | Polyurethane (1-component duroplastic) | 5,000 ± 1,000 mPa·s (DIN 53019, D=15 s-1, 23 °C) | 65 ± 10 min at 80 °C or 30 ± 5 min at 90 °C | -60 °C to +125 °C | – |
| PK 4344 | Polyurethane (1-component, heat-curing) | 2,000 ± 500 mPa·s (DIN 53019, D=15 s-1, 23 °C) | 65 ± 10 min at 80 °C or 30 ± 5 min at 90 °C | -60 °C to +125 °C | – |
| PK 4351 | Polyurethane (1-component) | 6,250 ± 1,250 mPa·s (DIN 53019, D=15 s-1, 23 °C) | 80 °C | -60 °C to +125 °C | – |
| PK 4353 | Polyurethane (1-component, heat-curing) | 3,500 ± 500 mPa·s (DIN 53019, D=15 s-1, 23 °C) | 60-70 min | -50 °C to +125 °C | – |
| PK 4364B | Liquid polyol system with encapsulated isocyanate hardener | – | 60-70 min | – | – |
| PK 5532 | Polyurethane elastomer (1-component) | 5,500 mPa·s | 30 minutes | -50 °C to +140 °C | – |
| PK 5542 | Polyurethane (1-component duroplastic) | 5,000 ± 1,000 mPa·s (DIN 53019, D=15 s-1, 23 °C) | 30 min | -50 °C to +140 °C | – |
| PK 5553 | Polyurethane (1-component) | 3,500 mPa·s | 90 °C | -50 °C to +130 °C | – |
| PT 4600 | Polyurethane, one-component, solvent-free | 400–900 mPa·s (23 °C, DIN 53229) | – | -40 to +125 °C | V-0 (File E211569, films of 10–55 µm only; not for the usual 200 µm film) |
| PT 4601 | Polyurethane, one-component, solvent-free, thixotropic | – | – | -40 to +120 °C | – |
| PT 4606 | Polyurethane (1-component, solvent-free) | 38,000 ± 8,000 mPa·s (DIN 53019, D = 10 s⁻¹, 23 °C) | – | -40 to +120 °C | – |
| PT 4700 N | Polyurethane (UV + moisture shadow-cure) | 200 ± 100 mPa·s (DIN 53019, 23 °C) | – | – | V-0 (ELANTAS internal test) |
| PT 4810 | Polyurethane | 3,500 mPa·s | – | -50 °C to +120 °C | – |
| PT 4810 N | Polyurethane | – | – | -50 °C to +100 °C | – |
| PT 4812 | Polyurethane | 2,600 mPa·s | – | -50 °C to +100 °C | – |
| PT 4812 N | Polyurethane | – | – | -50 °C to +100 °C | – |
| PT 4814 | Polyurethane | 1,400 ± 500 mPa·s | – | -50 °C to +100 °C | – |
| PT 4814 N | Polyurethane | – | – | -50 °C to +100 °C | – |
| PT 4830 | Polyurethane | 50,000 ± 10,000 mPa·s (DIN 53019, 23 °C, D = 15 s⁻¹) | – | -45 °C to +100 °C | – |
| PT 4832 | Polyurethane | 50,000 mPa·s | – | -45 °C to +100 °C | – |
| PT 4834 | Polyurethane | 3,200 ± 800 mPa·s | – | -45 °C to +100 °C | – |
| PT 4840 | Polyurethane | 125,000 mPa·s | – | -40 °C to +120 °C | – |
| PT 4842 | Polyurethane | 3,700 mPa·s | 2 days | -40 °C to +120 °C | – |
Also in this family, datasheet on request: PK 5540, PK 5560, PK 5562, PT 4605, PT 4810NV, PT 4812NV, PT 4814NV, SC 7575, SC 7576.
Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024). Datasheet PDFs.
Ask for a sample, a TDS, a quote or a dose calculation
Tell us what you need. We reply within 24 hours, in Romanian or English.
Contact directly
Alexandru Nichifor
Sales & technical support
nichiforlx@
Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298