Adhesives and sealants: 14 ELANTAS Bectron® materials
14 Bectron® adhesives and sealants from ELANTAS Europe, for fixing components and sealing housings and covers. The table gives base, viscosity, cure, operating temperature and UL 94 where the ELANTAS datasheet states them. Where a cell shows a dash, ask us for the TDS. For the neutral-cure SA 70 silicones, see Adhesives and sealants.
| Code | Base | Viscosity | Cure | Operating temperature | UL 94 |
|---|---|---|---|---|---|
| AR 4800 N | 1-component, moisture cure | 2,400 mPa·s | Tack-free 60–120 min; 24–48 h at room temperature, heat optional | -40 to +120 °C | – |
| AR 4820 N | One-component polyurethane, moisture cure | – | – | -45 to +120 °C | – |
| AR 4822 N | 1-component polyurethane, moisture cure | 15,000 ± 4,000 mPa·s (23 °C, D = 3 s⁻¹, DIN 53019) | 24 h at room temperature (≥ 50 % RH, up to 0.5 mm); for best adhesion 24 h at RT, then 24 h at 90 °C | -45 to +120 °C | – |
| AR 4826 N | 1-component, moisture cure, thixotropic | – | Tack-free 60–120 min; 24–48 h at room temperature, heat optional | -40 to +120 °C | – |
| EP 5611 | One-component modified epoxy, UV + heat dual cure, filled, thixotropic | 25,000–40,000 mPa·s (25 °C, DIN 53019, D = 50 s⁻¹) | UV 1–3 s at 50 mW/cm² UVA (+30 min at 150 °C); heat only 30 min at 150 °C | -40 to +150 °C (Insert 8, 09/2022) | – |
| EP 5620 | One-component modified epoxy, heat cure, solvent-free | 800 ± 300 mPa·s (23 °C, DIN 53019, D = 3 s⁻¹) | – | – | – |
| SA 70L1-30 | One-component condensation cure silicone (Alkoxy), neutral cure | 44,000 mPa·s | Tack-free 2–10 min (23 °C, 55 % RH); cured < 24 h (3 mm) | Temperature resistance -55 to +200 °C | – |
| SA 70L1-36 | Silicone (1-part) | 3,200 mPa·s | – | -40/+200 °C | – |
| SA 70P1-15 | Silicone (1-part) | Paste | – | -40 to +200 °C | – |
| SA 70P1-30 | Silicone (1-part) | Paste | 36 hours at 23 °C (3mm thickness) | -55 °C to +200 °C | – |
| SA 70P1-34 | Silicone (1-part) | Paste | – | -40 to +200 °C | – |
| SA 70P9-50 | Silicone | Paste | – | -55 to +160 °C | V-0 (File E140720, 3 and 5 mm) |
| SA 70P9-60 | Silicone (1-part) | Paste | 24 hours at 25 °C (3 mm thickness) | -55 °C to +200 °C | – |
| SA 70V1-36 | Silicone | – | – | -55 °C to +200 °C | – |
Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024). Datasheet PDFs.
Ask for a sample, a TDS, a quote or a dose calculation
Tell us what you need. We reply within 24 hours, in Romanian or English.
Contact directly
Alexandru Nichifor
Sales & technical support
nichiforlx@
Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298