Bectron® EP 5502
epoxy potting compound, ELANTAS Europe
Values from the ELANTAS brochure table. Ask for the current TDS before you specify the product.
| Chemical base | Epoxy |
|---|---|
| Colour | Transparent yellowish |
| Pot life | 30 min |
| Glass transition temperature | 70 °C |
| Operating temperature | Max. operation temperature +120 °C (no lower limit printed) |
| Hardener | EH 5908 |
Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).