Bectron® EP 5503

epoxy potting compound, ELANTAS Europe

Values from the ELANTAS brochure table. Ask for the current TDS before you specify the product.

Tab. 1Datasheet values: EP 5503
Chemical baseEpoxy resin
Viscosity6000 ± 1500 mPa*s
Mix ratio100:18-20 (by weight)
Cure18 h
Cure temperature23 °C
HardnessShore D 85
Dielectric strength32 kV/mm
Glass transition temperature122 °C
Operating temperature-40 °C to +150 °C
Water absorption0.7 %
HardenerEH 5908

Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).

Request TDS / SDS

Automotive control unit in a plastic housing, its circuit board encapsulated under clear potting compound
Image: ELANTAS Europe
Request TDS / SDS
Delivery
8 weeks from order
Documents
Certificate of analysis from ELANTAS

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice

Contact directly

Alexandru Nichifor
Sales & technical support

+40 771 709 622

nichiforlx@nalteksolutions.com

Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298