Bectron® EP 5611

adhesive / sealant, ELANTAS Europe

These values come from a preliminary ELANTAS datasheet. Ask for the current TDS before you qualify it.

Tab. 1Datasheet values: EP 5611
Chemical baseOne-component modified epoxy, UV + heat dual cure, filled, thixotropic
ColourPale white - grey
Viscosity25,000–40,000 mPa·s (25 °C, DIN 53019, D = 50 s⁻¹)
Density1.59–1.67 g/cm³ (25 °C, DIN 53217)
CureUV 1–3 s at 50 mW/cm² UVA (+30 min at 150 °C); heat only 30 min at 150 °C
Hardness85–95 Shore D (25 °C, ISO 868)
Dielectric strength25–29 kV/mm (23 °C, IEC 60455-2)
Thermal conductivity0.40–0.50 W/m·K (DIN 52613)
Glass transition temperature140–150 °C (TMA, 10 K/min)
Operating temperature-40 to +150 °C (Insert 8, 09/2022)
Shelf life12 months at < -18 °C (frozen product)

Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).

Request TDS / SDS

Formed-in-place gasket beads dispensed on a housing lid
Image: Naltek archive
Request SDS / sample
TDS
Technical data sheet (PDF)TDS N° 1168 Rev. 2, 10/2021 · 3 pages, 139 KBAll datasheets →
Delivery
8 weeks from order
Documents
Certificate of analysis from ELANTAS

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice

Contact directly

Alexandru Nichifor
Sales & technical support

+40 771 709 622

nichiforlx@nalteksolutions.com

Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298