| Chemical base | One-component modified epoxy, heat cure, solvent-free |
|---|---|
| Colour | Transparent |
| Viscosity | 800 ± 300 mPa·s (23 °C, DIN 53019, D = 3 s⁻¹) |
| Density | 1.1554 g/cm³ (20 °C, DIN EN ISO 2811-1) |
| Shelf life | 6 months at 5 °C or below |
Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).
Request TDS / SDS
- TDS
- Technical data sheet (PDF)06/12/2019 · 3 pages, 720 KBAll datasheets →
- Delivery
- 8 weeks from order
- Documents
- Certificate of analysis from ELANTAS
Application notes
Ask for a sample, a TDS, a quote or a dose calculation
Tell us what you need. We reply within 24 hours, in Romanian or English.
Contact directly
Alexandru Nichifor
Sales & technical support
nichiforlx@
Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298