Bectron® MR 3405 FR

hot-melt moulding resin, ELANTAS Europe

Values from the ELANTAS brochure table. Ask for the current TDS before you specify the product.

Tab. 1Datasheet values: MR 3405 FR
Chemical basePolyolefin
ColourBlack
Viscosity2,000 mPa·s @200 °C
Hardness35 A
UL 94V-0 (ELANTAS brochure)

Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).

Request TDS / SDS

Two test boards thick-film coated with Bectron® melting resin, translucent yellow-green and black
Image: ELANTAS Europe
Request TDS / SDS
Delivery
8 weeks from order
Documents
Certificate of analysis from ELANTAS

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice

Contact directly

Alexandru Nichifor
Sales & technical support

+40 771 709 622

nichiforlx@nalteksolutions.com

Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298