Bectron® PB 3201

polybutadiene potting compound, ELANTAS Europe

Tab. 1Datasheet values: PB 3201
Chemical basePolybutadiene
ColourWhite, milky
Viscosity7,500 ± 2,000 mPa·s (DIN 53019, D=7 s-1, 23 °C)
Density0.91 ± 0.05 g/cm³ (resin)
Mix ratio100:58 by weight (PB 3201 : PH 4918)
Pot life25 min
Cure48 h
Cure temperature>20 °C Room temperature; 60 °C
HardnessShore A 70 ± 10
Dielectric strength>30 kV/mm
Glass transition temperature-63 °C
Operating temperature-60 °C to +150 °C
Water absorption1.3 %
Shelf life6 months
HardenerPH 4918

Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).

Request TDS / SDS

Automotive control unit in a plastic housing, its circuit board encapsulated under clear potting compound
Image: ELANTAS Europe
Request SDS / sample
TDS
Technical data sheet (PDF)29/05/2008 · 3 pages, 154 KBAll datasheets →
Delivery
8 weeks from order
Documents
Certificate of analysis from ELANTAS

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice

Contact directly

Alexandru Nichifor
Sales & technical support

+40 771 709 622

nichiforlx@nalteksolutions.com

Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298