Bectron® PB 3251

polybutadiene potting compound, ELANTAS Europe

Tab. 1Datasheet values: PB 3251
Chemical basePolybutadiene
ColourBlack
Viscosity15000 ± 3000 mPa*s
Mix ratio100:33 (by weight)
Pot life20 min
Cure48 h
Hardness80 ± 10 Shore A
Glass transition temperature-63 °C
Operating temperature-60 to +150 °C
Elongation at break200 %
Water absorption0.3 %
HardenerPH 4918

Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).

Request TDS / SDS

Automotive control unit in a plastic housing, its circuit board encapsulated under clear potting compound
Image: ELANTAS Europe
Request SDS / sample
TDS
Technical data sheet (PDF)23/07/2013 · 3 pages, 109 KBAll datasheets →
Delivery
8 weeks from order
Documents
Certificate of analysis from ELANTAS

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice

Contact directly

Alexandru Nichifor
Sales & technical support

+40 771 709 622

nichiforlx@nalteksolutions.com

Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298