Bectron® PB 3252

polybutadiene potting compound, ELANTAS Europe

Values from the ELANTAS brochure table. Ask for the current TDS before you specify the product.

Tab. 1Datasheet values: PB 3252
Chemical basePolybutadiene
ColourBeige
Viscosity2000 ± 500 mPa*s
Mix ratio3:1 (by weight)
Pot life25 min
Cure48 h
HardnessShore A 65 ± 10
Dielectric strength13 kV/mm
Thermal conductivity0.20 W/m·K
Glass transition temperature-55 °C
Operating temperature-55 to +120 °C
Water absorption0.3 %

Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).

Request TDS / SDS

Automotive control unit in a plastic housing, its circuit board encapsulated under clear potting compound
Image: ELANTAS Europe
Request TDS / SDS
Delivery
8 weeks from order
Documents
Certificate of analysis from ELANTAS

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice

Contact directly

Alexandru Nichifor
Sales & technical support

+40 771 709 622

nichiforlx@nalteksolutions.com

Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298