Bectron® PH 4913
hardener, ELANTAS Europe
| Chemical base | Polyurethane hardener (filled PU casting compounds) |
|---|---|
| Colour | Brown transparent |
| Viscosity | 27.5 ± 12.5 mPa·s (25 °C, DIN 53019) |
| Density | 1.21 ± 0.05 g/cm³ (20 °C, DIN EN ISO 2811-2) |
| Shelf life | 6 months (23 °C) |
Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).