Bectron® PK 4332
thick-film conformal coating, ELANTAS Europe
| Chemical base | Polyurethane (1-component) |
|---|---|
| Colour | black |
| Viscosity | 5,500 ± 1,000 mPa·s (DIN 53019, D=15 s-1, 23 °C) |
| Density | 1.05 ± 0.03 g/cm³ (DIN EN ISO 2811-2, 23 °C) |
| Cure | 70-90 min |
| Cure temperature | 80 °C |
| Hardness | 35 ± 10 Shore A (ISO 868, 23 °C) |
| Dielectric strength | 22 kV/mm |
| Thermal conductivity | 0.18 ± 0.02 W/mK (DIN 52616, 23 °C) |
| Glass transition temperature | -50 °C (IEC 61006) |
| Operating temperature | -60 °C to +125 °C |
| Shelf life | 7 months |
Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).
Request TDS / SDS
- TDS
- Technical data sheet (PDF)07/02/2012 · 3 pages, 93 KBAll datasheets →
- Delivery
- 8 weeks from order
- Documents
- Certificate of analysis from ELANTAS
Application notes
Ask for a sample, a TDS, a quote or a dose calculation
Tell us what you need. We reply within 24 hours, in Romanian or English.
Contact directly
Alexandru Nichifor
Sales & technical support
nichiforlx@
Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298