Bectron® PK 4344

thick-film conformal coating, ELANTAS Europe

Tab. 1Datasheet values: PK 4344
Chemical basePolyurethane (1-component, heat-curing)
ColourBlack
Viscosity2,000 ± 500 mPa·s (DIN 53019, D=15 s-1, 23 °C)
Density1.28 ± 0.01 g/cm³ (DIN 51757, 23 °C)
Cure65 ± 10 min at 80 °C or 30 ± 5 min at 90 °C
Cure temperature80 °C
Hardness70 Shore A
Dielectric strength22 kV/mm
Thermal conductivity0.18 ± 0.02 W/mK (DIN 52616, 23 °C)
Glass transition temperature-50 °C
Operating temperature-60 °C to +125 °C
Shelf life6 months (23 °C)

Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).

Request TDS / SDS

Control unit in its housing, divided into zones showing thin film coating, thick film coating and encapsulation/potting
Image: ELANTAS Europe
Request SDS / sample
TDS
Technical data sheet (PDF)14/09/2016 · 3 pages, 245 KBAll datasheets →
Delivery
8 weeks from order
Documents
Certificate of analysis from ELANTAS

Application notes

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice

Contact directly

Alexandru Nichifor
Sales & technical support

+40 771 709 622

nichiforlx@nalteksolutions.com

Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298