Bectron® PK 5532
thick-film conformal coating, ELANTAS Europe
Values from the ELANTAS brochure table. Ask for the current TDS before you specify the product.
| Chemical base | Polyurethane elastomer (1-component) |
|---|---|
| Colour | Black |
| Viscosity | 5,500 mPa·s |
| Density | 1.010 to 1.110 g/cm³ |
| Solids content | 100% |
| Cure | 30 minutes |
| Cure temperature | +90 °C |
| Hardness | 35 Shore A |
| Dielectric strength | 9 kV/mm |
| Thermal conductivity | 0.2 W/m·K |
| Glass transition temperature | Below -60 °C |
| Operating temperature | -50 °C to +140 °C |
| Max. temperature (20,000 h) | +125 °C (20,000 h) |
Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).
Request TDS / SDS
- Delivery
- 8 weeks from order
- Documents
- Certificate of analysis from ELANTAS
Application notes
Ask for a sample, a TDS, a quote or a dose calculation
Tell us what you need. We reply within 24 hours, in Romanian or English.
Contact directly
Alexandru Nichifor
Sales & technical support
nichiforlx@
Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298