Bectron® PK 5553

thick-film conformal coating, ELANTAS Europe

Values from the ELANTAS brochure table. Ask for the current TDS before you specify the product.

Tab. 1Datasheet values: PK 5553
Chemical basePolyurethane (1-component)
ColourBlack
Viscosity3,500 mPa·s
Density1.140 to 1.240 g/cm³
Solids content100%
Cure temperature90 °C
Hardness30 Shore D
Dielectric strength9 kV/mm
Thermal conductivity0.3 W/mK
Glass transition temperatureBelow -60 °C
Operating temperature-50 °C to +130 °C

Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).

Request TDS / SDS

Control unit in its housing, divided into zones showing thin film coating, thick film coating and encapsulation/potting
Image: ELANTAS Europe
Request TDS / SDS
Delivery
8 weeks from order
Documents
Certificate of analysis from ELANTAS

Application notes

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice

Contact directly

Alexandru Nichifor
Sales & technical support

+40 771 709 622

nichiforlx@nalteksolutions.com

Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298