Bectron® PL 1102
thin-film conformal coating, ELANTAS Europe
| Chemical base | Acrylic |
|---|---|
| Colour | Transparent |
| Viscosity | 40 ± 15 s, 4 mm cup, 23 °C (≈ 50 mPa·s) |
| Dielectric strength | > 156 kV/mm (23 °C); > 120 kV/mm after 23 h in water (IEC 60464-2) |
| Operating temperature | Temperature resistance 130 °C |
| UL 94 | V-0 (ELANTAS internal test) |
Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).
Request TDS / SDS
- TDS
- Technical data sheet (PDF)25/05/2018 · 3 pages, 668 KBAll datasheets →
- Delivery
- 8 weeks from order
- Documents
- Certificate of analysis from ELANTAS
Application notes
Ask for a sample, a TDS, a quote or a dose calculation
Tell us what you need. We reply within 24 hours, in Romanian or English.
Contact directly
Alexandru Nichifor
Sales & technical support
nichiforlx@
Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298