Bectron® PL 1104

thin-film conformal coating, ELANTAS Europe

Tab. 1Datasheet values: PL 1104
Chemical baseAcrylic
ColourTransparent
Viscosity40 ± 15 seconds flow time (DIN/EN/ISO 2431, 4mm cup, 23 °C) ≈ 50 mPa·s
Density0.90 ± 0.01 g/cm³ (DIN 51757, 23 °C)
Solids content20.5 ± 1% (ISO 3251, 1.5g, 1h, 110 °C)
Dielectric strength>156 kV/mm (IEC 60464, 23 °C)
Operating temperature-40 °C to +130 °C
Water absorption4.5 mg (ISO 62, 23 °C, 24 h)
Shelf life12 months at 23 °C

Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).

Request TDS / SDS

Control unit in its housing, divided into zones showing thin film coating, thick film coating and encapsulation/potting
Image: ELANTAS Europe
Request SDS / sample
TDS
Technical data sheet (PDF)18/08/2016 · 3 pages, 295 KBAll datasheets →
Delivery
8 weeks from order
Documents
Certificate of analysis from ELANTAS

Application notes

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice

Contact directly

Alexandru Nichifor
Sales & technical support

+40 771 709 622

nichiforlx@nalteksolutions.com

Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298