Bectron® PL 4122-37
thin-film conformal coating, ELANTAS Europe
| Chemical base | Polyurethane varnish |
|---|---|
| Colour | Transparent |
| Viscosity | 40 ± 3 seconds (DIN/EN/ISO 2431, 4mm cup, 23 °C) ≈ 50 mPa·s |
| Density | 0.86 ± 0.01 g/cm³ (DIN EN ISO 2811-2, 23 °C) |
| Solids content | 37 ± 1% (ISO 3251, 1.5g, 2h, 130 °C) |
| Dielectric strength | 112 kV/mm |
| Operating temperature | Temperature index 134 °C (IEC 60216) |
| Water absorption | 1.5 % |
| Shelf life | 6 months (-10 to 25 °C IBC/drum; 0 to 25 °C tins up to 25 kg) |
| UL 94 | V-0 (File E211569) |
| Pack size | 0.4 kg can; 4 kg can |
Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).
Request TDS / SDS
- TDS
- Technical data sheet (PDF)27/02/2024 · 3 pages, 664 KBAll datasheets →
- Delivery
- 8 weeks from order
- Documents
- Certificate of analysis from ELANTAS
Application notes
Ask for a sample, a TDS, a quote or a dose calculation
Tell us what you need. We reply within 24 hours, in Romanian or English.
Contact directly
Alexandru Nichifor
Sales & technical support
nichiforlx@
Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298