Bectron® PL 5621D

thin-film conformal coating, ELANTAS Europe

Tab. 1Datasheet values: PL 5621D
Chemical baseEpoxy
Viscosity400 ± 250 mPa·s (DIN 53019)
UV doseUVA (315–380 nm) 1,500 mJ/cm², or 30 min at 90 °C
Dielectric strength165 kV/mm (150 after 24 h in water)
Operating temperature-40 to +130 °C (short-term 160 °C)
Shelf life3 months at 5 °C
UL 94V-0 (ELANTAS internal test)

Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).

Request TDS / SDS

Control unit in its housing, divided into zones showing thin film coating, thick film coating and encapsulation/potting
Image: ELANTAS Europe
Request SDS / sample
TDS
Technical data sheet (PDF)18/08/2016 · 3 pages, 283 KBAll datasheets →
Delivery
8 weeks from order
Documents
Certificate of analysis from ELANTAS

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice

Contact directly

Alexandru Nichifor
Sales & technical support

+40 771 709 622

nichiforlx@nalteksolutions.com

Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298