Bectron® PT 4810
thick-film conformal coating, ELANTAS Europe
Values from the ELANTAS brochure table. Ask for the current TDS before you specify the product.
| Chemical base | Polyurethane |
|---|---|
| Viscosity | 3,500 mPa·s |
| Hardness | 45 Shore A |
| Operating temperature | -50 °C to +120 °C |
| Max. temperature (20,000 h) | +100 °C (20,000 h) |
Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).
Request TDS / SDS
- Delivery
- 8 weeks from order
- Documents
- Certificate of analysis from ELANTAS
Application notes
Ask for a sample, a TDS, a quote or a dose calculation
Tell us what you need. We reply within 24 hours, in Romanian or English.
Contact directly
Alexandru Nichifor
Sales & technical support
nichiforlx@
Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298