Bectron® PT 4812
thick-film conformal coating, ELANTAS Europe
| Chemical base | Polyurethane |
|---|---|
| Viscosity | 2,600 mPa·s |
| Hardness | 40 Shore A |
| Operating temperature | -50 °C to +100 °C |
Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).