Bectron® PT 4842
thick-film conformal coating, ELANTAS Europe
| Chemical base | Polyurethane |
|---|---|
| Colour | Transparent clear |
| Viscosity | 3,700 mPa·s |
| Density | 1.12 ± 0.05 g/cm³ |
| Cure | 2 days |
| Hardness | 45 Shore A |
| Dielectric strength | 20 kV/mm |
| Operating temperature | -40 °C to +120 °C |
| Elongation at break | 270 % |
| Water absorption | 0.2 % |
Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).
Request TDS / SDS
- TDS
- Technical data sheet (PDF)27/02/2024 · 3 pages, 625 KBAll datasheets →
- Delivery
- 8 weeks from order
- Documents
- Certificate of analysis from ELANTAS