Bectron® PU 4501
polyurethane potting compound, ELANTAS Europe
| Chemical base | Polyurethane (2-part, polyetherpolyol resin + aliphatic isocyanate hardener) |
|---|---|
| Colour | Transparent clear |
| Mix ratio | 100:50 (by weight) |
| Pot life | 35 min |
| Hardness | 35 ± 10 Shore A |
| Dielectric strength | 73 kV/mm |
| Thermal conductivity | 0.16 to 0.20 W/m·K |
| Glass transition temperature | -40 °C |
| Operating temperature | Temperature cycling -40/+125 °C |
| Hardener | PH 4901 |
Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).
Request TDS / SDS
- TDS
- Technical data sheet (PDF)30/07/2013 · 3 pages, 117 KBAll datasheets →
- Delivery
- 8 weeks from order
- Documents
- Certificate of analysis from ELANTAS
Application notes
Ask for a sample, a TDS, a quote or a dose calculation
Tell us what you need. We reply within 24 hours, in Romanian or English.
Contact directly
Alexandru Nichifor
Sales & technical support
nichiforlx@
Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298