Bectron® PU 4528
polyurethane potting compound, ELANTAS Europe
Values from the ELANTAS brochure table. Ask for availability and the current TDS before you specify the product.
| Chemical base | Polyurethane (PU) |
|---|---|
| Colour | Transparent yellow |
| Viscosity | 4,000 mPa·s |
| Pot life | 25 min |
| Hardness | 20 Shore A |
| Hardener | PH 4915 |
Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).