Bectron® SA 70P1-30
adhesive / sealant, ELANTAS Europe
| Chemical base | Silicone (1-part) |
|---|---|
| Colour | Translucent |
| Viscosity | Paste |
| Density | 1.08-1.13 g/cm³ |
| Cure | 36 hours at 23 °C (3mm thickness) |
| Hardness | 25-35 Shore A |
| Operating temperature | -55 °C to +200 °C |
| Elongation at break | 545% |
| Tensile strength | 2.43 MPa |