Bectron® SA 70P9-60
adhesive / sealant, ELANTAS Europe
Values from the ELANTAS brochure table. Ask for availability and the current TDS before you specify the product.
| Chemical base | Silicone (1-part) |
|---|---|
| Colour | Black |
| Viscosity | Paste |
| Density | 1.25 g/cm³ |
| Cure | 24 hours at 25 °C (3 mm thickness) |
| Hardness | 60 Shore A |
| Operating temperature | -55 °C to +200 °C |
| Elongation at break | 200% |
| Tensile strength | 2.35 MPa |
Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).