Bectron® SA 70V1-36
adhesive / sealant, ELANTAS Europe
Values from the ELANTAS brochure table. Ask for the current TDS before you specify the product.
| Chemical base | Silicone |
|---|---|
| Colour | translucent |
| Hardness | Shore A 36 |
| Operating temperature | -55 °C to +200 °C |
| Elongation at break | 141 % |
| Tensile strength | 1.52 MPa |
| Pack size | 0.320 kg |
Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).