| Chemical base | Silicone Gel (2-component) |
|---|---|
| Colour | Transparent |
| Viscosity | 350 mPa·s |
| Pot life | 120 minutes at 25 °C |
| Cure | 24 h |
| Dielectric strength | >10 kV/mm |
| Thermal conductivity | 0.20 W/m*K |
| Glass transition temperature | < -40 °C |
| Operating temperature | -45 to +200 °C |
| UL 94 | V-1 (ELANTAS internal test) |
| Hardener | SG 79V1-60 |
Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).
Request TDS / SDS
- Delivery
- 8 weeks from order
- Documents
- Certificate of analysis from ELANTAS
Application notes
Ask for a sample, a TDS, a quote or a dose calculation
Tell us what you need. We reply within 24 hours, in Romanian or English.
Contact directly
Alexandru Nichifor
Sales & technical support
nichiforlx@
Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298