Bectron® SG 75V1-75
silicone gel, ELANTAS Europe
| Chemical base | Silicone (2-component, addition cure) |
|---|---|
| Colour | Transparent (both components) |
| Viscosity | 750–1,250 mPa·s mixed (25 °C) |
| Density | 0.96 g/cm³ (SG 75V1-75), 0.97 g/cm³ (SG 79V1-75), 23 °C |
| Mix ratio | 1:1 by weight |
| Pot life | 45 minutes at room temperature |
| Cure | 1.5 h at room temperature; 15 min at 60 °C; 5.5 min at 120 °C |
| Dielectric strength | >10 kV/mm |
| Thermal conductivity | 0.20 W/m*K |
| Glass transition temperature | < -40 °C |
| Operating temperature | -40 °C to +180 °C |
| UL 94 | HB (File E140720, 3 mm) |
| Hardener | SG 79V1-75 |
Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).
Request TDS / SDS
- TDS
- Technical data sheet (PDF)TDS N° 1813 Rev. 2, 01/2024 · 4 pages, 177 KBAll datasheets →
- Delivery
- 8 weeks from order
- Documents
- Certificate of analysis from ELANTAS
Application notes
Ask for a sample, a TDS, a quote or a dose calculation
Tell us what you need. We reply within 24 hours, in Romanian or English.
Contact directly
Alexandru Nichifor
Sales & technical support
nichiforlx@
Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298