Bectron® SK 76V2-50
silicone potting elastomer, ELANTAS Europe
Values from the ELANTAS brochure table. Ask for the current TDS before you specify the product.
| Chemical base | Silicone (2-component) |
|---|---|
| Colour | Beige-Blue (resin / hardener) |
| Viscosity | 2,600 mPa·s |
| Solids content | 100% |
| Pot life | 30 min |
| Cure | 24 h |
| Hardness | 50 Shore A |
| Dielectric strength | 24 kV/mm |
| Thermal conductivity | 0.4 W/mK |
| Glass transition temperature | < -40 °C |
| Operating temperature | -40 to +180 °C |
| Max. temperature (20,000 h) | 180 °C |
| Hardener | SH 79V5-50 |
Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).
Request TDS / SDS
- Delivery
- 8 weeks from order
- Documents
- Certificate of analysis from ELANTAS
Application notes
Ask for a sample, a TDS, a quote or a dose calculation
Tell us what you need. We reply within 24 hours, in Romanian or English.
Contact directly
Alexandru Nichifor
Sales & technical support
nichiforlx@
Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298