Bectron® SK 76V2-75

silicone potting elastomer, ELANTAS Europe

Tab. 1Datasheet values: SK 76V2-75
Chemical baseSilicone (2-component, condensation cure)
ColourBeige (base) / Blue (hardener)
Viscosity7,500 mPa·s at 25 °C
Density1.56 g/cm³ (20 °C)
Mix ratio100 parts SK 76V2-75 : 2.5 parts SH 79V5-75 (by weight)
Pot life20 minutes at room temperature
Cure6 h
HardnessShore A 75
Dielectric strength<30 kV/mm
Thermal conductivity0.42 W/m*K
Glass transition temperature< -40 °C
Operating temperature-40 °C to +180 °C
UL 94V-1
HardenerSH 79V5-75

Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).

Request TDS / SDS

Automotive control unit in a plastic housing, its circuit board encapsulated under clear potting compound
Image: ELANTAS Europe
Request SDS / sample
TDS
Technical data sheet (PDF)26/04/2017 · 3 pages, 249 KBAll datasheets →
Delivery
8 weeks from order
Documents
Certificate of analysis from ELANTAS

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice

Contact directly

Alexandru Nichifor
Sales & technical support

+40 771 709 622

nichiforlx@nalteksolutions.com

Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298