Hoenle LED Powerline LC (with LED Powerdrive)
Line · LED UV curing, Hoenle AG
Water-cooled UV-LED line array; lengths up to 3,000 mm on request; clean-room suitable.
| Wavelengths | 365 / 385 / 395 / 405 nm |
|---|---|
| Irradiance | 365: 14,000 | 385: 20,000 | 395: 25,000 | 405: 25,000 mW/cm² (typical; Hoenle LED sensors for the UV Meter; Hoenle states no distance) |
| Emission window | irradiation width 76–3,000 mm; other lengths up to 3,000 mm on request |
| Cooling | water cooled |
| Control and interfaces | 0-10 V analog dimming; digital PLC (emergency-stop, LED-on, LED failure, temperature warning); LED Powerdrive tabletop controller |
Wavelength against the band in the TDS
The PL 5621 D TDS names UVA 315–380 nm. Pick one of this unit’s wavelengths.
The emission peak is schematic. Sources: Hoenle AG; ELANTAS TDS PL 5621 D.
Typical applications according to Hoenle: curing UV / visible-light adhesives, coatings, sealants, high-speed inkjet printing (original design), clean-room processes.
Source: Hoenle product flyer (PDF, updated 09/25) · hoenle.com
Hoenle LED Powerline LC (with LED Powerdrive)
- Lead time
- Hoenle AG standard units, accessories and spare parts: about 4–5 weeks from order. Custom systems: lead time per quote. We agree the delivery terms with you for each order.
Line: LED Powerline ACIC (with LED Powerdrive IC) · LED Line 500
Ask for a sample, a TDS, a quote or a dose calculation
Tell us what you need. We reply within 24 hours, in Romanian or English.
Contact directly
Alexandru Nichifor
Sales & technical support
nichiforlx@
Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298