Bectron® MR 3406 FR

hot-melt moulding resin, ELANTAS Europe

These values come from a preliminary ELANTAS datasheet. Ask for the current TDS before you qualify it.

Tab. 1Datasheet values: MR 3406 FR
Chemical baseHydrocarbon melting resin, polyolefin-based (1-component)
ColourBlack
Viscosity800–1,250 mPa·s (180 °C, PP 25, DIN 53019)
Density0.84–0.86 g/cm³ (23 °C, DIN 16945)
Hardness15–25 Shore A (23 °C, ISO 868)
Dielectric strength> 9 kV/mm (23 °C, IEC 60455-2)
Operating temperature-40 to +125 °C (max. operation temperature 125 °C, 168 h)
Shelf life12 months (5–35 °C)
UL 94V-0

Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).

Request TDS / SDS

Two test boards thick-film coated with Bectron® melting resin, translucent yellow-green and black
Image: ELANTAS Europe
Request SDS / sample
TDS
Technical data sheet (PDF)TDS N° 1926 Rev. 2, 03/2024 · 3 pages, 137 KBAll datasheets →
Delivery
8 weeks from order
Documents
Certificate of analysis from ELANTAS

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice

Contact directly

Alexandru Nichifor
Sales & technical support

+40 771 709 622

nichiforlx@nalteksolutions.com

Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298