Bectron® PU 4513

polyurethane potting compound, ELANTAS Europe

Tab. 1Datasheet values: PU 4513
Chemical basePolyurethane (2-component, solvent-free)
ColourDark Blue
Viscosity750 ± 150 mPa·s (DIN 53019, 25 °C)
Density1.40 ± 0.05 g/cm³ (DIN EN ISO 2811-1, 20 °C)
Mix ratio3.5 : 1 (by volume); 4.0 : 1 (by weight)
Pot life50 min
Cure24 h at room temperature or 1–1.5 h at 90 °C
Hardness79 ± 9 Shore A
Dielectric strength22 kV/mm
Thermal conductivity0.36 W/m·K
Glass transition temperature-10 °C
Operating temperatureThermal class 115 °C (IEC 216); flexible down to -40 °C
Tensile strength3.01 MPa
Water absorption0.36 %
Shelf life6 months
HardenerPH 4912

Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).

Request TDS / SDS

Automotive control unit in a plastic housing, its circuit board encapsulated under clear potting compound
Image: ELANTAS Europe
Request SDS / sample
TDS
Technical data sheet (PDF)10/03/2008 · 3 pages, 162 KBAll datasheets →
Delivery
8 weeks from order
Documents
Certificate of analysis from ELANTAS

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice

Contact directly

Alexandru Nichifor
Sales & technical support

+40 771 709 622

nichiforlx@nalteksolutions.com

Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298