Bectron® PH 4912

hardener, ELANTAS Europe

Hardener for Bectron® polyurethane potting compounds, among them PU 4522 and PU 4526. Use up an opened container as soon as possible: moisture in the air reduces reactivity.

Tab. 1Datasheet values: PH 4912
Chemical basePolyurethane hardener
ColourAmber
Viscosity90–140 mPa·s (25 °C, ISO 3219)
Density1.22–1.26 g/ml (25 °C, ASTM D 1475)
Shelf life6 months

Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).

Request TDS / SDS

Request TDS / SDS
Delivery
8 weeks from order
Documents
Certificate of analysis from ELANTAS

Hardeners, thinners and cleaners

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice

Contact directly

Alexandru Nichifor
Sales & technical support

+40 771 709 622

nichiforlx@nalteksolutions.com

Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298