polyurethane potting compound, ELANTAS Europe
| Chemical base | Polyurethane (2-component) |
|---|---|
| Colour | Black |
| Viscosity | 310 ± 90 mPa·s (DIN 53019, 25 °C) |
| Density | 1.03 ± 0.05 g/cm³ (DIN EN ISO 2811-1, 20 °C) |
| Pot life | 26 min |
| Cure | 36h @RT, 1h @90 °C |
| Hardness | 70 ± 10 Shore D (ISO 868) |
| Thermal conductivity | 0.215 ± 0.015 W/mK |
| Shelf life | 6 months |
| Hardener | PH 4912 |
Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).
Request TDS / SDS
- TDS
- Technical data sheet (PDF)31/08/2010 · 3 pages, 80 KBAll datasheets →
- Delivery
- 8 weeks from order
- Documents
- Certificate of analysis from ELANTAS
Application notes
Ask for a sample, a TDS, a quote or a dose calculation
Tell us what you need. We reply within 24 hours, in Romanian or English.
Contact directly
Alexandru Nichifor
Sales & technical support
nichiforlx@
Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298