Bectron® PU 4522
polyurethane potting compound, ELANTAS Europe
| Chemical base | Polyurethane (2-component liquid) |
|---|---|
| Viscosity | 1,800 ± 300 mPa·s mixed, 25 °C (resin 3,500 ± 300) |
| Density | 1.50 ± 0.05 g/cm³ |
| Mix ratio | 100 : 15 by weight = 5.4 : 1 by volume (20 °C), with PH 4912 |
| Pot life | 15–20 min (25 °C) |
| Cure | 6–8 h at room temperature or 0.5 h at 90 °C |
| Hardness | 85 ± 5 Shore A |
| Dielectric strength | 18 kV/mm |
| Glass transition temperature | -22 °C |
| Operating temperature | -40 °C to +125 °C |
| Water absorption | 0.4 % |
| Shelf life | 6 months |
| UL 94 | V-0 |
| Hardener | PH 4912 |
Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).
Request TDS / SDS
- TDS
- Technical data sheet (PDF)01/10/2012 · 3 pages, 120 KBAll datasheets →
- Delivery
- 8 weeks from order
- Documents
- Certificate of analysis from ELANTAS
Application notes
Ask for a sample, a TDS, a quote or a dose calculation
Tell us what you need. We reply within 24 hours, in Romanian or English.
Contact directly
Alexandru Nichifor
Sales & technical support
nichiforlx@
Naltek Solutions S.R.L.