Bectron® SK 75V2-65
silicone potting elastomer, ELANTAS Europe
| Chemical base | Silicone (2-component, addition cure) |
|---|---|
| Colour | Beige (both components) |
| Viscosity | 3,500 mPa·s at 25 °C |
| Density | 1.78 g/cm³ (20 °C) |
| Mix ratio | 1:1 (parts by weight) |
| Pot life | 60 minutes at room temperature |
| Cure | 24 h |
| Hardness | 50–80 Shore A, typical 65 (DIN 53505, 16 h at 80 °C) |
| Dielectric strength | 11 kV/mm |
| Thermal conductivity | 0.45 W/m*K |
| Glass transition temperature | < -40 °C |
| Operating temperature | -40 °C to +200 °C |
| UL 94 | V-0 (ELANTAS internal test) |
| Hardener | SH 79V2-65 |
Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).
Request TDS / SDS
- TDS
- Technical data sheet (PDF)26/04/2017 · 3 pages, 352 KBAll datasheets →
- Delivery
- 8 weeks from order
- Documents
- Certificate of analysis from ELANTAS
Ask for a sample, a TDS, a quote or a dose calculation
Tell us what you need. We reply within 24 hours, in Romanian or English.
Contact directly
Alexandru Nichifor
Sales & technical support
nichiforlx@
Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298