UV dose calculator
Pick the material and the lamp, set power and belt speed. The calculator checks the dose against the datasheet window and tells you which speed or power lands in the middle of it.
05,808 mJ/cm²
5,280 mJ/cm²
Above the window: overdose
TDS window: 2,500–3,500 mJ/cm²
For the middle of the window (3,000 mJ/cm²): belt at 4.4 m/min at this power, or 57 % power at this speed.
- The TDS names only the band (UVA), no wavelength. The LED’s suitability is confirmed in a trial.
Assumptions
- Dose scales linearly with power; Hoenle does not state this.
- Catalogue irradiance is Hoenle’s typical value, Hoenle: “measured with Hoenle LED sensors for UV meter” (Hoenle states no measuring distance).
- Working distance enters only through the measured value above; distance curves come from Hoenle (v2).
- Time under the lamp = window length along the belt ÷ belt speed. Length along the belt: window as printed: “82 x 20 or 122 x 20” mm; Short side of the window, i.e. the lamp mounted across the belt. Hoenle does not state the mounting orientation; this is a Naltek assumption printed under the result.
Sources
- PT 4600: 2500 - 3500 mJ / cm² (UVA) [ELANTAS Bectron® PT 4600 TDS, p. 3]
- Hoenle LED Powerline ACIC – ACIC 820 XP, 82 × 20 mm: 365 nm column of the typical-intensity row “11.000 16.000 16.000 22.000” (mW/cm²) [Hoenle AG flyer, LED Powerline ACIC, p. 2]
- Length along the belt: window as printed: “82 x 20 or 122 x 20” mm; Short side of the window, i.e. the lamp mounted across the belt. Hoenle does not state the mounting orientation; this is a Naltek assumption printed under the result. [Hoenle AG flyer, LED Powerline ACIC, p. 2]
- Power: between 10 % and 100 % in 1 %-steps. [Hoenle AG flyer, LED Powerline ACIC, p. 2]
- PT 4600: blue → green/yellow [ELANTAS Bectron® PT 4600 TDS, p. 2]