Bectron® PT 4600

thick-film conformal coating, ELANTAS Europe

Tab. 1Datasheet values: PT 4600
Chemical basePolyurethane, one-component, solvent-free
ColourTransparent blue; turns green/yellow as it UV-cures
Viscosity400–900 mPa·s (23 °C, DIN 53229)
Density1.06–1.16 g/cm³ (23 °C, ISO 2811-2)
UV doseUVA 2,500–3,500 mJ/cm², 3–7 s (about 5 s at 3,000 mJ/cm² for a 200 ± 50 µm film)
Hardness60–70 Shore A (23 °C, ISO 868)
Dielectric strength70–80 kV/mm (23 °C, IEC 60464-2)
Glass transition temperature-15 to -20 °C (IEC 61006)
Operating temperature-40 to +125 °C
Shelf life6 months at +5 to +10 °C (cartridge, bladder bag) or -10 to +25 °C (steel pail)
UL 94V-0 (File E211569, films of 10–55 µm only; not for the usual 200 µm film)

Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).

Request TDS / SDS

Control unit in its housing, divided into zones showing thin film coating, thick film coating and encapsulation/potting
Image: ELANTAS Europe
Request SDS / sample
TDS
Technical data sheet (PDF)TDS N° 1875 Rev. 2, 02/2024 · 3 pages, 137 KBAll datasheets →
Delivery
8 weeks from order
Documents
Certificate of analysis from ELANTAS

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice

Contact directly

Alexandru Nichifor
Sales & technical support

+40 771 709 622

nichiforlx@nalteksolutions.com

Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298