Bectron® PU 4526

polyurethane potting compound, ELANTAS Europe

Tab. 1Datasheet values: PU 4526
Chemical baseTwo-component polyurethane, with Hardener Bectron PH 4912
ColourBlack
Viscosity3,000–4,000 mPa·s mixed, 25 °C (resin 10,000–18,000)
Density1.52–1.58 g/ml resin (25 °C, ASTM D 1475); cured 1.47–1.53
Mix ratio100 : 16.6 by weight; 100 : 21.5 by volume, with PH 4912
Pot life12–22 min (25 °C)
Hardness35–45 Shore D/15 (25 °C, ASTM D 2240)
Dielectric strength22–26 kV/mm (25 °C, 2 mm, ASTM D 149)
Thermal conductivity0.55–0.70 W/m·K (25 °C, ASTM C 518)
Glass transition temperature5–15 °C (ASTM D 3418)
Operating temperature-30 to +130 °C
Elongation at break50–70 % (25 °C, ASTM D 638)
Tensile strength4.0–5.0 MPa (25 °C, ASTM D 638)
Water absorption0.10–0.20 % (24 h RT, ASTM D 570)
Shelf life6 months
UL 94V-0 (File E116643, 5.5 mm)
HardenerPH 4912

Manufactured by ELANTAS Europe; ELANTAS Europe’s plants are certified to IATF 16949:2016 (ELANTAS presentation, 07/2024).

Request TDS / SDS

Automotive control unit in a plastic housing, its circuit board encapsulated under clear potting compound
Image: ELANTAS Europe
Request SDS / sample
TDS
Technical data sheet (PDF)TDS N° 2121 Rev. 4, 12/2024 · 4 pages, 178 KBAll datasheets →
Delivery
8 weeks from order
Documents
Certificate of analysis from ELANTAS

Ask for a sample, a TDS, a quote or a dose calculation

Tell us what you need. We reply within 24 hours, in Romanian or English.

What do you need?

The button opens your email program with the inquiry filled in; you send it from there. We use these details only to answer this inquiry. Privacy notice

Contact directly

Alexandru Nichifor
Sales & technical support

+40 771 709 622

nichiforlx@nalteksolutions.com

Naltek Solutions S.R.L.
Sat Comori, Com. Gurghiu, nr. 81, jud. Mureș 547298